1) Waya wa Iron Chrome Aluminium
CrAl 14-4, CrAl 15-5, CrAl 20-5, CrAl 25-5, etc.
2) Nichrome Waya
NiCr 80/20, NiCr 70/30, NiCr 60/15, NiCr 35/20
3) Nickel Copper Alloy Waya
Aloyi 30, Aloyi 60, Aloyi 90, Constantan Waya
Kuti mumve zambiri, pls pitani patsamba lathu kapena titumizireni imelo.
MFUNDO:
1Cr13Al4 | 0.03-12.0 | 1.25±0.08 | 588-735 | > 16 | > 6 | 950 | > 10000 |
0Cr15Al5 | 1.25±0.08 | 588-735 | > 16 | > 6 | 1000 | > 10000 | |
0Cr25Al5 | 1.42±0.07 | 634-784 | > 12 | >5 | 1300 | > 8000 | |
0Cr23Al5 | 1.35±0.06 | 634-784 | > 12 | >5 | 1250 | > 8000 | |
0Cr21Al6 | 1.42±0.07 | 634-784 | > 12 | >5 | 1300 | > 8000 | |
1Cr20Al3 | 1.23±0.06 | 634-784 | > 12 | >5 | 1100 | > 8000 | |
Mtengo wa 0Cr21Al6Nb | 1.45±0.07 | 634-784 | > 12 | >5 | 1350 | > 8000 | |
Chithunzi cha 0Cr27Al7Mo2 | 0.03-12.0 | 1.53±0.07 | 686-784 | > 12 | >5 | 1400 | > 8000 |
Kufunika:
Fecrak ife aloyi yabwino yokhala ndi kukana kwenikweni kwenikweni (1.20-1.30 ohm-mm2/m) yomwe imaphatikiza kukana kutentha mpaka 1450C ndipo imanenedwa kuti ndiyofunikira pakutentha kwambiri. . Ili ndi kukana kwabwino kwa dzimbiri pamlengalenga, mu argon, mu vacuum, oxidizing, okhala ndi sulfure komanso malo a carboniferous. Imawonetsa kusachulukira kwakukulu (7.2g/cm3), koma imakhala ndi malire okolola.
Mtengo wa Cr15Al5 Eurofechral
zakuthupi | kalasi | Dzina la UNS | DIN | Kuchulukana | Chithunzi cha ASTM |
fecral | 1.4725 | K92500 | 17470 | 7.4 | Chithunzi cha 603-1 |
Ntchito zazikulu:ng'anjos, zinthu zopinga, ng'anjo zotentha kwambiri, zinthu zotenthetsera zama tubula ndi ma heaters.
Maperesenti:
Al | Cr | Fe | Mn | C | Si | Ni | Cu | Ti | Zina | Zosowa zapadziko lapansi |
4.6-5.8 | 14.5-15.5 | Maziko | Zokwanira 0.7 | mpaka 0.05 | mpaka 0.6 | mpaka 0.6 | … | mpaka 0.6 | Zr≤0.3 | … |
Mawonekedwe Amakina T°20°C
Chiwerengero cha mawerama | Peresenti yowonjezera |
>5 nthawi | >16% |
Mawonekedwe a Thupi T°20°C
Kuuma | Kuchulukana | Kuthyola katundu | Maximum Ntchito kutentha 850C | Kulimbana ndi magetsi | Magnetism | Malo osungunuka (°C) |
200-260 HB | 7.1g/cm3 | 637-784m/pa | 1.30 ohn-mm2/m | Maginito | 1400 ° C |