| Gulu | Ndi% | Ku% | Al% | Ti% | Fe% | Mn% | S% | C% | Si% |
| Ndalama K500 | mphindi 63 | 27.0-33.0 | 2.30-3.15 | 0.35-0.85 | Kuchuluka kwa 2.0 | Zokwanira 1.5 | Kuchuluka kwa 0.01 | Kuchuluka kwa 0.25 | Kuchuluka kwa 0.5 |
Zofotokozera
| Fomu | Standard |
| Monel K-500 | UNS N05500 |
| Malo | Chithunzi cha ASTM B865 |
| Waya | AMS4676 |
| Mapepala/Mbale | Chithunzi cha ASTM B865 |
| Kupanga | Chithunzi cha ASTM B564 |
| Weld Waya | ERNiCu-7 |
Zakuthupi(20°C)
| Gulu | Kuchulukana | Melting Point | Kukaniza Magetsi | Kutanthauza Coefficient of Thermal Expansion | Thermal Conductivity | Kutentha Kwapadera |
| Ndalama K500 | 8.55g/cm3 | 1315°C-1350°C | 0.615 μΩ•m | 13.7(100°C) a/10-6°C-1 | 19.4(100°C) λ/(W/m•°C) | 418 J/kg•°C |
Mechanical Properties(20°C Mphindi)
| Monel K-500 | Kulimba kwamakokedwe | Kupambana Kwambiri RP0.2% | Elongation A5% |
| Annealed & Aged | Min. 896 pa | Min. 586MPa | 30-20 |