Kufotokozera
Nickel Alloy Monel K-500, aloyi yowumitsa zaka, yomwe ili ndi aluminiyamu ndi titaniyamu, imaphatikiza mawonekedwe abwino kwambiri okana dzimbiri a Monel 400 ndi mapindu owonjezera amphamvu, amaumitsa, ndikusunga mphamvu zake mpaka 600 ° C.
Kukana kwa dzimbiri kwa Monel K-500 kumakhala kofanana ndi kwa Monel 400 kupatula kuti, mumkhalidwe woumitsidwa ndi ukalamba, Monel K-500 imatha kukhudzidwa ndi kupsinjika-kusweka kwa dzimbiri m'malo ena.
Zina mwazomwe zimagwiritsidwa ntchito ndi nickel alloy K-500 ndi zida zapampu, zoyikapo, masamba azachipatala ndi scrapers, makola obowola mafuta, ndi zida zina zomalizitsira, zida zamagetsi, akasupe ndi masitima apamtunda. Alloy iyi imagwiritsidwa ntchito makamaka m'mafakitale am'madzi ndi mafuta ndi gasi. Mosiyana ndi Monel 400 ndi yosunthika kwambiri, kupeza ntchito zambiri pamadenga, ngalande, ndi zida zomanga panyumba zingapo zamabungwe, machubu otenthetsera madzi otentha, kugwiritsa ntchito madzi am'nyanja (sheathing, ena), njira ya HF alkylation, kupanga ndi kusamalira HF. asidi, ndi kuyenga uranium, distillation, mayunitsi condensation, ndi pamwamba condenser mapaipi mu zoyenga ndi mafakitale petrochemical, ndi ena ambiri.
Chemical Composition
Gulu | Ndi% | Ku% | Al% | Ti% | Fe% | Mn% | S% | C% | Si% |
Ndalama K500 | mphindi 63 | 27.0-33.0 | 2.30-3.15 | 0.35-0.85 | Kuchuluka kwa 2.0 | Max 1.5 | Kuchuluka kwa 0.01 | Kuchuluka kwa 0.25 | Kuchuluka kwa 0.5 |
Zofotokozera
Fomu | Standard |
Monel K-500 | UNS N05500 |
Malo | Chithunzi cha ASTM B865 |
Waya | AMS4676 |
Mapepala/Mbale | Chithunzi cha ASTM B865 |
Kupanga | Chithunzi cha ASTM B564 |
Weld Waya | ERNiCu-7 |
Zakuthupi(20°C)
Gulu | Kuchulukana | Melting Point | Kukaniza Magetsi | Kutanthauza Coefficient of Thermal Expansion | Thermal Conductivity | Kutentha Kwapadera |
Ndalama K500 | 8.55g/cm3 | 1315°C-1350°C | 0.615 μΩ•m | 13.7(100°C) a/10-6°C-1 | 19.4(100°C) λ/(W/m•°C) | 418 J/kg•°C |
Mechanical Properties(20°C Mphindi)
Monel K-500 | Kulimba kwamakokedwe | Kupambana Kwambiri RP0.2% | Elongation A5% |
Annealed & Aged | Min. 896 pa | Min. 586MPa | 30-20 |