Ubwino wathu: Wapamwamba kwambiri, nthawi yochepa yobereka, MOQ yaying'ono.
Mawonekedwe: Kuchita kokhazikika; Anti-oxidation; Kukana dzimbiri; Kukhazikika kwa kutentha kwakukulu; Kukhoza kwabwino kupanga koyilo; Uniform komanso kukongola kwa pamwamba popanda mawanga.
Kagwiritsidwe:Kukana Kutentha zinthu; Zida mu zitsulo; Zipangizo zapakhomo; Kupanga kwamakina ndi mafakitale ena.
Gulu | Ni80Cr20 | Ni70Cr30 | Ni60Cr23 | Ni60Cr15 | Ni35Cr20 | Karma | Evanohm | |
Zolemba mwadzina% | Ni | Bali | Bali | 58.0-63.0 | 55.0-61.0 | 34.0-37.0 | Bali | Bali |
Cr | 20.0-23.0 | 28.0-31.0 | 21.0-25.0 | 15.0-18.0 | 18.0-21.0 | 19.0-21.5 | 19.0-21.5 | |
Fe | ≦1.0 | ≦1.0 | Bali | Bali | Bali | 2.0-3.0 | - | |
Al1.0-1.7 Ti 0.3-0.5 | Al2.7-3.2 Mn0.5-1.5 | Al2.7-3.2 Cu2.0-3.0 Mn0.5-1.5 | ||||||
Kutentha kwambiri (°C) | 1200 | 1250 | 1150 | 1150 | 1100 | 300 | 400 | |
Resisivity(Ω/cmf,20℃) | 1.09 | 1.18 | 1.21 | 1.11 | 1.04 | 1.33 | 1.33 | |
Kukanika (uΩ/m, 60°F) | 655 | 704 | 727 | 668 | 626 | 800 | 800 | |
Kachulukidwe (g/cm³) | 8.4 | 8.1 | 8.4 | 8.2 | 7.9 | 8.1 | 8.1 | |
Thermal Conductivity(KJ/m·h·℃) | 60.3 | 45.2 | 45.2 | 45.2 | 43.8 | 46.0 | 46.0 | |
Linear Expansion Coefficient(×10¯6/ ℃) 20-1000 ℃) | 18.0 | 17.0 | 17.0 | 17.0 | 19.0 | - | - | |
Malo osungunuka (℃) | 1400 | 1380 | 1370 | 1390 | 1390 | 1400 | 1400 | |
Kulimba (Hv) | 180 | 185 | 185 | 180 | 180 | 180 | 180 | |
Kulimbitsa Mphamvu (N/mm2 ) | 750 | 875 | 800 | 750 | 750 | 780 | 780 | |
Kutalikira (%) | ≥20 | ≥20 | ≥20 | ≥20 | ≥20 | 10-20 | 10-20 | |
Kapangidwe ka Micrographic | austenite | austenite | austenite | austenite | austenite | austenite | austenite | |
MagneticProperty | Ayi | Ayi | Ayi | Pang'ono | Ayi | Ayi | Ayi | |
Moyo Wofulumira (h/℃) | ≥81/1200 | ≥50/1250 | ≥81/1200 | ≥81/1200 | ≥81/1200 | - | - |